Atomic Layer Deposition on Nanoporous Atomically Thin Membranes to Tune Pore Sizes

Researchers

Rohit N Karnik / Lohyun Kim / Simar Mattewal

Departments: Department of Mechanical Engineering, Chemical Engineering
Technology Areas: Chemicals & Materials: Composites, Nanotechnology & Nanomaterials / Energy & Distribution: Electrochemical Devices / Environmental Engineering: Water Treatment

  • membranes including atomic layer deposition treated atomically thin active layers